Carpet foam mixed latex
Details

Carpet foam mixed latex consists of three components: material A, B and C:

-Material A: A mixture of natural latex and synthetic latex, and the main ingredients are latex, fillers, stabilizers, antioxidants, and foaming agents

-Material B: vulcanization system water dispersion, the main component is vulcanization agent, main facilitator.

-Material C: Casing agent, including gel setting agent, gel setting promoting agent.

 

Performance parameters for the item A components

the name of a shop

Solid content (%)

PH price

Viscosity (cp, rotor # 5,100rpm)

pigment

Product wear resistance

CF20

70-71

10-11

1100-1300

ivory

outstanding

CF30

71-72

10-11

1100-1300

ivory

fine

CF40

71-72

10-11

1200-1400

ivory

same as

 

Performance parameters of item B, component C

Indicator project

B material

C material

Solid content (%)

50

30-45

PH price

10-11

10-11

Viscosity (cp, 100rpm)

600-800

15

pigment

buff

 Colourless clarification

 

Note: Materials A, B shall be stirred for 10-15 minutes before use. Avoid sunlight exposure during storage, and the storage temperature is at 5-35.

 

Recommended use ratio

the name of a shop

Item A dosage

Item B dosage

Material C dosage

CF20

100

5.0-5.5

4

CF30

100

4.0-4.5

4

CF40

100

3.5-4.0

4

 

matters need attention:

Materials A and B are fully stirred evenly before use, which is very important for the stability of product quality. Please follow it.

 

 Suggestions:

1.  The temperature of the sulfide package is controlled within 130 degrees, which is of great help to the wear resistance of the product.

2. The air volume of the vulcanized oven has a great influence on the vulcanization speed. It is suggested that customers should increase the air volume and reduce the temperature so as to get the best wear resistance of the product.